MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Toyobo Pibiflex® E5578FR01 Thermoplastic Copolyester Elastomer
Categories: Polymer; Thermoplastic; Polyester, TP; Polyester Thermoplastic Elastomer

Material Notes: Product Description: Pibiflex E5578FR01 a nominal 58 Shore D thermoplastic polyester elastomer that is V-2 flame retardant. This grade is appropriate for extrusion applications.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Good Heat Resistance

Additive: Flame Retardant

Features: Flame Retardant

Processing Method: Extrusion

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.26 g/cc0.0455 lb/in³ISO 1183
Maximum Moisture Content 0.0500.050
Melt Flow 19 g/10 min
@Load 2.16 kg,
Temperature 230 °C
19 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 58
@Time 15.0 sec
58
@Time 0.00417 hour
ISO 868
Tensile Strength at Break 29.0 MPa4210 psiISO 37
Elongation at Break >= 300 %>= 300 %ISO 37
Flexural Modulus 0.250 GPa36.3 ksiISO 178
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 V-2
@Thickness 1.52 mm
V-2
@Thickness 0.0600 in
 
Processing PropertiesMetricEnglishComments
Drying Temperature 100 - 110 °C212 - 230 °F
Dry Time 4.00 hour4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHCQ6311 / 311004

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.