Applications: Used for flame retardancy, smoke suppression, and antimony trioxide replacement in rigid and flexible PVC compounds. Key Benefits: - Highly effective Fire-Retardant additive for Flexible & Rigid PVC applications.
- Fire retardant with excellent LOI performance.
Information provided by J.M. Huber Corporation |