MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Outokumpu 4303 Cr-Ni Austenitic Stainless Steel
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel

Material Notes: Good corrosion resistance with excellent drawing properties.

Applications: Suitable for cold formed components where good workability is required. Fasteners, studs.

Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms.

Key Words: EN 1.4303; ASTM 305; JIS SUS 305J1
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.90 g/ccRT
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 570 MPaOutokumpu Typical, Cold Rolled Narrow Strip; EN 10002-1
Tensile Strength, Yield 220 MPa
@Strain 0.2 %
EN min., RT; EN 10002-1
 250 MPa
@Strain 0.2 %
Outokumpu Typical,Cold Rolled Narrow Strip; EN 10002-1
 280 MPa
@Strain 1 %
Outokumpu Typical,Cold Rolled Narrow Strip; EN 10002-1
 98.0 MPa
@Strain 0.2 %,
Temperature 400 °C
EN min.; EN 10002-5
 127 MPa
@Strain 0.2 %,
Temperature 200 °C
EN min.; EN 10002-5
 155 MPa
@Strain 0.2 %,
Temperature 100 °C
EN min.; EN 10002-5
Elongation at Break 50 %Outokumpu Typical, Cold Rolled Narrow Strip; EN 10002-1
Modulus of Elasticity 200 GPaRT
 172 GPa
@Temperature 400 °C
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000730 ohm-cmRT
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.0 µm/m-°C
@Temperature 100 °C
 17.5 µm/m-°C
@Temperature 400 °C
Specific Heat Capacity 0.500 J/g-°CRT
Thermal Conductivity 15.0 W/m-KRT
 20.0 W/m-K
@Temperature 400 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.040 %
Chromium, Cr 17.7 %
Iron, Fe 69.76 %
Nickel, Ni 12.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
305 Stainless Steel, annealed, sheet
Cast Stainless Steel 440C, JIS G4303
Outokumpu 4301 Cr-Ni Austenitic Stainless Steel
AK Steel 305 Austenitic Stainless steel
305 Stainless Steel, annealed, strip

NOUTOK18 / 18733

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.