MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Top Polymer Topolymer® 5711-851M TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Production Description: Topolymer® 5711-M is a kind of halogen-free flame-retardant compound which made from SEBS (styrene isoprene/butadiene block copolymer), It was designed specially for parts and cables with requirement of halogen-free flame-retardant.

Features: Excellent flexibility, Good hand feel, Pass the UL94-V0 standard

Information provided by Top Polymer Enterprise

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.03 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 85
Tensile Strength 110 kg(f)/cm²
Elongation at Break 400 %
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 120 - 160 °CInjection
Middle Barrel Temperature 180 - 220 °CInjection
Front Barrel Temperature 180 - 220 °CInjection
Nozzle Temperature 160 - 200 °CInjection
Mold Temperature 40.0 - 60.0 °CInjection
Injection Pressure 3.00 - 10.0 MPaInjection
Screw Speed 30 - 80 rpmInjection
 
Descriptive Properties
ColorNatural
Screw L/D22:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Top Polymer Topolymer® 5711-651M TPE
Top Polymer Topolymer® 5711-951M TPE
Top Polymer Topolymer® 5711-801M TPE
Advanced Elastomer Systems Santoprene® 283-40 Thermoplastic Rubber

PTOPO026 / 184538

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.