MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teijin Panlite® G-3130PH Glass Fiber Reinforced Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 30% Glass Filled

Material Notes: Glass Fiber Reinforcement grades-30% glass fiber, high appearance camera grade. Availability: Africa, Middle East, Asia Pacific, Europe, Latin America, North America. Filter / reinforcement: Glass fiber, 30% filler by weight. Features: Creep resistant, High rigidity, good surface finish, Low Anisotropy. Uses: Camera Applications. Forms: pellets. Processing Method: Injection Molding.

Information provided by Teijin Chemicals Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.43 g/ccISO 1183
Moisture Absorption 0.120 %
@Temperature 23.0 °C,
Time 86400 sec
ISO 62
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm
@Thickness 4.00 mm
Teijin method
Linear Mold Shrinkage, Transverse 0.0030 - 0.0050 cm/cm
@Thickness 4.00 mm
Teijin method
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 86.0 MPaISO 527-2/5
Elongation at Break 2.0 %ISO 527-2/5
Tensile Modulus 5000 MPaISO 527-2/1
Flexural Strength 135 MPa2.0 mm/min; ISO 178
Flexural Modulus 6000 MPa2.0 mm/min; ISO 178
Charpy Impact Unnotched 38.0 kJ/m²ISO 179
Charpy Impact, Notched 10.0 kJ/m²ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmIEC 60093
Dielectric Constant 3.5
@Frequency 100 Hz
IEC 60250
 3.5
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 35.0 kV/mmshort time test; IEC 60243-1
Dissipation Factor 0.0010
@Frequency 100 Hz
IEC 60250
 0.0090
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 175 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 30.0 µm/m-°CISO 11359-2
CTE, linear, Transverse to Flow 60.0 µm/m-°CISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 134 °Cunannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 126 °Cunannealed; ISO 75-2/A
Vicat Softening Point 138 °CISO 306/B50
UL RTI, Electrical 80.0 °C
@Thickness 1.70 mm
UL 746
UL RTI, Mechanical with Impact 80.0 °C
@Thickness 1.70 mm
UL 746
UL RTI, Mechanical without Impact 80.0 °C
@Thickness 1.70 mm
UL 746
Flammability, UL94 V-2
@Thickness 1.70 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Teijin Panlite® G-3420H Glass Fiber Reinforced Polycarbonate
Teijin Panlite® G-3420R Glass Fiber Reinforced Polycarbonate Resin
E-Glass Fiber, Generic
DuPont™ Kevlar® Aramid Pulp
DuPont™ Kevlar® 29 Aramid Fiber

PTEIH950 / 191635

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.