MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Avient OnForce™ LFT PP-50LGF/001 Natural Polypropylene Homopolymer (PP Homopolymer)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. These products exhibit enhanced physical and mechanical properties versus standard short fiber products. Benefits of LFT compounds include improved impact strength, elastic modulus, and material strength across wide temperature ranges from subambient to highly elevated. Furthermore, LFT compounds have been shown to offer improved performance in the areas of creep and fatigue performance, improved dimensional stability, and exhibit an exceptional surface finish when compared to traditional highly filled short fiber products.

LFT compounds can be processed using equipment similar to that used for short fiber products. The mechanical properties of finished parts depend greatly on the length of the fibers in the molded part; therefore processing conditions must be set carefully in order to minimize fiber breakage. A low shear process is advised, with low back pressure, low screw speed and low-to-medium injection speed.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.30 g/ccISO 1183
Filler Content 50 %Long Glass Fiber
Linear Mold Shrinkage 0.0030 cm/cmMeasured on a tensile specimen.; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 130 MPaISO 527-2
Elongation at Break 2.0 %ISO 527-2
Tensile Modulus 12000 MPaISO 527-2
Flexural Strength 180 MPaISO 178
Flexural Modulus 9000 MPaISO 178
Charpy Impact Unnotched 60.0 kJ/m²ISO 179
Charpy Impact, Notched 25.0 kJ/m²ISO 179
Gardner Impact 11.9 JASTM D5420
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 152 °CUnannealed; ISO 75-2/A
Deflection Temperature at 8.0 MPa 144 °CUnannealed; ISO 75-2/C
 
Processing PropertiesOriginal ValueComments
Melt Temperature 210 - 230 °C
Mold Temperature 60.0 °C
Drying Temperature 80.0 °C
Dry Time 2.00 hour
Back Pressure 1.00 MPa
 
Descriptive Properties
FeaturesHeat Stabilized
FormsPellets
Generic MaterialPP Homopolymer
Generic NamePolypropylene Homopolymer (PP Homopolymer)
Injection RateSlow-Moderate
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
PlastiComp Complet® LGF40 - PP Homopolymer Polypropylene, 40% Long Glass Fiber Reinforced
Avient OnForce™ LFT NN-50LGF/000 HS Black Polyamide 66 (Nylon 66)
Avient OnForce™ LFT PP-60LGF/001 Natural Polypropylene Homopolymer (PP Homopolymer)
PlastiComp Complet® LGF50 - PP Homopolymer Polypropylene, 50% Long Glass Fiber Reinforced
Avient OnForce™ LFT PP-30LGF/001 Natural Polypropylene Homopolymer (PP Homopolymer)

PH0POL1376 / 145945

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.