MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Astro Met AmAlOx 87 Alumina - Aluminum Oxide
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: AmAlOx 87 alumina (Astro Met Aluminum Oxide) is a 99.95% alumina ceramic manufactured by Astro Met for specialty applications which require a higher purity of alumina than found in commercial grades of 99.5% and 99.8% alumina. AmAlOx 87 alumina is especially cost effective for applications, which need the unique combination of high purity, high strength, high density and small grain size in one material.

AmAlOx 87 alumina, originally developed for critical load bearing medical implants, has an unusually small grain size for an alumina ceramic, this enables extremely tight tolerances and surface finishes of 2 microinches Ra to be achieved when proper finishing techniques are used.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 3.97 g/cc
Particle Size 2.0 µm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 2000
Flexural Strength 482 MPa
 
Component Elements PropertiesOriginal ValueComments
Al2O3 99.95 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CeramTec ATZ Alumina Toughened Zirconia, Dental Grade
Ferro Zirmonite 200, ZTA
CeramTec Rubalit® HSS Alumina, 75% (High Strength Substrate)
CeramTec Rubalit® 708 HP Alumina, 96% (High Performance)
CeramTec Ceramtape GC Glass Ceramic

CASTR01 / 629

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.