MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Tra-Con Tra-Duct 921M01 Low Viscosity Long Pot Life Silver-Filled Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy, Electrically Conductive; Filled/Reinforced Thermoset

Material Notes: TRA-DUCT 921M01 is a two component, silver-filled electrically conductive epoxy adhesive designed for applications which require electrical conductivity and a long pot life at a relatively low heat cure. This adhesive is a soft, smooth paste ideal for application by automatic dispenser, screen-printing, or hand probe. This material can be conveniently packaged in our custom bipax as well as pre-mixed and frozen syringes.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 3.61 g/ccCured
Viscosity 23000 cPMixed (cp #52, 10 rpm)
 
Mechanical PropertiesOriginal ValueComments
Adhesive Bond Strength 1500 psiLap shear, alum to alum
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.00017 ohm-cmcured 15 min @ 150°C
 0.00025 ohm-cmcured 30 min @ 120°C
 0.00051 ohm-cmcured 2 hrs @ 80°C
 0.0041 ohm-cmcured 24 hrs @ 65°C
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 105 °CUltimate Tg
 
Processing PropertiesOriginal ValueComments
Cure Time 5.00 - 7.00 hour
@Temperature 80.0 °C
 15.0 min
@Temperature 150 °C
 24.0 hour
@Temperature 65.0 °C
 30.0 min
@Temperature 120 °C
 
Descriptive Properties
Color Silver
Thixotropic Index 4
Working Life days 2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTRAC193 / 71121

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.