System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Universal Wire Works Greek Ascoloy (AMS 5817) Filler Metal
Categories:
Metal
;
Ferrous Metal
;
Stainless Steel
;
Superalloy
;
Iron Base
Material Notes:
Greek Ascoloy is primarily used for gas metal arc and gas tungsten arc welding of corrosion resistant steels of similar composition.
Information provided by Universal Wire Works for their line of welding wire and filler metal.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Component Elements Properties
Original Value
Comments
Aluminum, Al
<= 0.15 %
Carbon, C
<= 0.20 %
Chromium, Cr
13 %
Copper, Cu
<= 0.50 %
Iron, Fe
>= 79.5 %
As Remainder
Manganese, Mn
<= 0.50 %
Molybdenum, Mo
<= 0.50 %
Nickel, Ni
2.0 %
Phosphorus, P
<= 0.040 %
Silicon, Si
<= 0.50 %
Sulfur, S
<= 0.030 %
Tin, Sn
<= 0.050 %
Tungsten, W
3.0 %
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
ATI Allvac® Vasco® Greek Ascoloy Specialty Steel, Heat Treatment: 871°C (1600°F) + Age
MetalTek MTEK CA20NW Cast UNS J91631 Martensitic Stainless Steel
Industeel SUPERELSO® 890 HLE Steel for Welded and Weight-Saving Structures
CBS-600 Carburizing Bearing and Gear Steel
Cast Stainless Steel 5342, UNS J92200
NUWW318 / 19745
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.