MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chemours Viton® A-100 with VC50+VC20 Fluoroelastomer Compound
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes:
  • Ultralow viscosity
  • Improved processing
  • increased mold flow
  • can be blended with other Viton® types to enhance processibility and improve flow
  • Excellent mold release
  • Good compression set resistance for low-viscosity types of Viton®

Applications

  • Transfer and injection molding of complex shapes such as gaskets
  • Extrusions can be used to modify viscosity of other types of Viton®
  • Solution coating for fabric and tanks or chemical containers

Chemours was formed from former DuPont performance chemicals businesses, including the Viton product line, in 2015.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Mooney Viscosity 27
@Temperature 121 °C
ML (1+10), Uncompounded Viton; ASTM D1646
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 5624 hours Postcure; ASTM D2240
 68No Postcure; ASTM D2240
Tensile Strength at Break 8.00 MPaNo Postcure; ASTM D412
 10.2 MPa24 hours Postcure; ASTM D412
Elongation at Break 242 %24 hours Postcure; ASTM D412
 296 %No Postcure; ASTM D412
100% Modulus 0.00270 GPa
@Strain 100 %
No Postcure; ASTM D1414
 0.00340 GPa
@Strain 100 %
24 hours Postcure; ASTM D1414
Compression Set 16 %
@Temperature 23.0 °C,
Time 252000 sec
O-Rings; ASTM D395B
 23 %
@Temperature 232 °C,
Time 79200 sec
O-Rings; ASTM D395B
 26 %
@Temperature 200 °C,
Time 252000 sec
O-Rings; ASTM D395B
 
Processing PropertiesOriginal ValueComments
Processing Temperature 177 °C
@Time 601 sec
Cure
 232 °C
@Time 86400 sec
Postcure
 
Descriptive Properties
Formulation as Tested0.3Viton® Curative #20
 2Viton® Curative #50
 25MT Black
 3MgO
 6Ca(OH)2
 97.5A-100

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chemours Viton® A-200 with Blanc Fixe Fluoroelastomer Compound
Chemours Viton® A-200 with Celite 350 Fluoroelastomer Compound
Chemours Viton® 40 Process Aid
Chemours Viton® 10 Process Aid
Chemours Viton® A-200 (97.5 phr) Formulation

PDVC9868 / 170509

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.