MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

BCC Products DP-11-88 Urethane Adhesive
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Adhesive

Material Notes: DP-11-88 is a medium viscosity quick setting easy to use urethane adhesive. This system was specifically designed to bond together the MB2001/MB3000 Model/Tooling Board to create desired dimensions in length, width, and height. Handling Properties: DP-11-88 Urethane Adhesive is a quick-setting, two part casting system which requires careful preparation prior to mixing parts A and B. Because DP-11-88 contains components having very low density, there will be some separation at the surface of the material in its container. Using a paint shaker, jiffy mixer, or mixing spatula, resuspension of the ingredients is easily accomplished. Precaution should be taken to prevent any moisture contamination from containers or utensils. It is recommended that the work area be well ventilated and normal cleanliness and safety rules be observed. Avoid prolonged exposure to vapors and contact with skin. Preparation of Mold Surface for Casting Applications: Clean the surface from dust and possible presence of moisture. Apply BC 87 Parting Agent and polish to a uniform high gloss finish (usually 2-3 coats are recommended). For wood surfaces, 2-3 coats of a quality sanding sealer is necessary. For plaster surfaces, seal with PVC sealer to ensure complete absence of moisture. For both wood and plaster surfaces, follow with 2-3 coats of BC 87 Parting Agent. Mixing and Pouring for Casting Applications: Pour weighted or measured amounts of Part A & B into a separate dry container by pouring Part A into Part B. Mix with a spatula or mechanical stirrer for 1 minute for quart size batches or 1 1/2 - 2 minutes for gallon batches. Immediately pour mixed resin uninterrupted from a convenient height above the mold cavity to resist air bubble entrapment. Clean the mixing tools by rinsing in an alcohol type solvent. Larger masses (2 feet or more) may be built up with successive pours. Castings may be demolded within 2 to 3 hours but should be properly supported while "green". Under normal conditions, maximum hardness or cure will be achieved in 12-18 hours.

Information provided by BCC Products, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.780 g/cc0.780 g/ccASTM-D-792-66
Brookfield Viscosity 3000 cP3000 cPPart A; ASTM D2393
 3750 cP3750 cPMixed, 1 minute; ASTM D2393
 4500 cP4500 cPPart B; ASTM D2393
Linear Mold Shrinkage 0.0010 cm/cm0.0010 in/inASTM D2566-69
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6262ASTM D2240
Tensile Strength, Ultimate 14.9 MPa2160 psiASTM-D-638
Flexural Strength 23.4 MPa3400 psiASTM D790
Flexural Modulus 1.16 GPa168 ksiASTM-D-790
Compressive Strength 19.13 MPa2775 psiASTM D695
Izod Impact, Notched 1.29 J/cm2.41 ft-lb/in
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 62.8 °C145 °FASTM-D-648-56
 
Processing PropertiesMetricEnglishComments
Cure Time 480 - 720 min
@Temperature 24.0 °C
8.00 - 12.0 hour
@Temperature 75.2 °F
demold time
Pot Life 10 - 12 min
@Temperature 24.0 °C
10 - 12 min
@Temperature 75.2 °F
ASTM-D-2471, 1/2lb mass
Gel Time 12.0 - 14.0 min12.0 - 14.0 minASTM-D-2471
 
Descriptive Properties
Mix Ratio1:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aptek UVISTAKE 7206 UV Curing, Urethane staking compound
Aptek UVISTAKE 7205LM-PMF UV Curing, Low Outgassing, Urethane staking compound
General Plastics LAST-A-FOAM® TF-6070-8.5 Polyurethane Foam
Covestro DUREFLEX® PS5400 TPU
Coastal Enterprises Plus™ PBHT-15 High Density Urethane Foam

PBCC011 / 107238

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.