2% Vinyl Acetate EVA copolymer and FDA compliant Features: High clarity film with good stiffness and low temperature toughness. Applications: Film extrusion: food packaging, general purpose packaging that requires low temperature toughness. FDA Notes: Conforms to FDA regulation 21 CFR 177.1350 under condition of use C through G described in Table 2 of 21 CFR 176.170 Film properties based on 1.0 guage (25 µm) thickness; blow-up ratio 2:1. Information provided by Huntsman Corporation |
Poly(Ethylene Vinyl Acetate) |