SABIC® PP 512MN10 has excellent flow properties and a good combination of high impact strength and stiffness. It is widely
used in articles where good processability, high toughness and a low warpage are required, e.g. vacuum-cleaner
housings, large size flower pots, foodstuff containers and ice-cream containers.
The product mentioned herein is in particular not tested and therefore not validated for use in pharmaceutical/
medical applications.
This grade material is UL registered under File E111275. IMDS 80775790Information provided by SABIC |