MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
EMS-Grivory Grilon® AG-35 PA66-GF35
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Glass Fiber Filled

Material Notes: Product description: Grilon AG-35 is a heat stabilized, normal viscosity PA 66 injection molding grade with 35% glass fibers.
  • High stiffness
  • High tensile strength
  • High heat distortion temperature
  • Easy processing
Application examples are stressed functional parts such as wheels, electrical bobbins, handles, levers and housings.

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.39 g/ccDry; ISO 1183
Water Absorption 5.0 %Sim. to ISO 62
Moisture Absorption 1.50 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0060 cm/cmISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 145 MPaConditioned; ISO 2039-1
 245 MPaDry; ISO 2039-1
Tensile Strength at Break 140 MPaConditioned; ISO 527-1/-2
 200 MPaDry; ISO 527-1/-2
Elongation at Break 3.0 %Dry; ISO 527-1/-2
 5.0 %Conditioned; ISO 527-1/-2
Tensile Modulus 8500 MPaConditioned; ISO 527-1/-2
 12500 MPaDry; ISO 527-1/-2
Charpy Impact Unnotched 75.0 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/1eU
 80.0 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eU
 85.0 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eU
 90.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eU
Charpy Impact, Notched 10.0 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/1eA
 10.0 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eA
 10.0 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eA
 15.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+10 ohm-cmConditioned; IEC 60093
 1.00e+12 ohm-cmDry; IEC 60093
Surface Resistance 1.00e+11 ohmIEC 60093
Dielectric Strength 38.0 kV/mmConditioned; IEC 60243-1
 41.0 kV/mmDry; IEC 60243-1
Comparative Tracking Index 600 VConditioned; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 20.0 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 100 µm/m-°CISO 11359-1/-2
Melting Point 260 °C10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 90.0 - 120 °CLong Term; ISO 2578
 200 °CShort Term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 250 °CISO 75-1/-2
Deflection Temperature at 8.0 MPa 165 °CISO 75-1/-2
Flammability, UL94 HBIEC 60695-11-10
 
Descriptive Properties
AutomotiveAutomotive electr. and electronics, lighting
 Powertrain and Chassis
Electricals & ElectronicsElectrical appliances
FormGranules
Industry & Consumer goodsHeating systems
 Mechanical Engineering
 Power transmission
 Sports & Leisure
 Tools & Accessories
ProcessingInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
EMS-Grivory Grilon® AS V0 PA66
EMS-Grivory Grilon® AG-25 HM PA66-GF25
DuPont Mobility and Materials Zytel® FG70G50HSLA BK309 PA66-GF50
Envalior Akulon® S223-HG7 PA66-GF35, Dry, 35% Glass Filled, Heat Stabilized
Celanese Zytel® 70G35EF NC010 PA66-GF35

PGRH154 / 156863

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.