MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
PSM Industries PolyAlloys MIM-Fe-%3Si Grade 2 Soft Magnetic Steel
Categories: Metal; Electronic/Magnetic Alloy

Material Notes: PolyAlloys Injected Metals, a division of PSM Industries, Inc., offers precision, High-Performance components for structural, magnetic and electronic applications that require a high degree of complexity and near full theoretical density by utilizing Metal Injection Molding (MIM).  MIM can economically produce complex shapes beyond the capability of conventional Powdered Metallurgy.
    Benefits of Metal Injection Molding
  • 96-98% of Theoretical Density
  • Excellent Mechanical Properties
  • Avoids Costly Secondary Operations
  • Excellent Surface Finishes
  • Capable of Extreme 3-D Geometries
  • Holds Tight Tolerances
  • Extremely Thin Wall Section Capabilities

Information Provided by PolyAlloys, a division of PSM Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.45 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 80Macro
Tensile Strength, Ultimate 77.0 ksi
Tensile Strength, Yield 57.0 ksi
@Strain 0.2 %
Elongation at Yield 24 %in 1 in.
 
Electrical PropertiesOriginal ValueComments
Magnetic Permeability >= 5500
 6000Typical
Magnetic Coercive Force, Hc 1.0 Oe
Magnetic Remanence, Br 12000 Gauss
 
Descriptive Properties
B25 (kG)14min
 14.5Typical
B500 (kG)19.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
PSM Industries PolyAlloys MIM-Fe-%3Si Grade 1 Soft Magnetic Steel
PSM Industries PolyAlloys MIM-316L sintered Stainless Steel
Kinetics MIM 2.5% SiFe Soft Magnetic Steel
PSM Industries PolyAlloys MIM-430L sintered Soft Magnetic Steel
Aluminum 384.0-F Die Casting Alloy

NPSM013 / 93204

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.