MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Bayport Polymers Baystar™ D4720 High Density Polyethylene Film Resin
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Medium Density (MDPE); Medium Density Polyethylene (MDPE), Film Grade

Material Notes: Medium Molecular Weight. Excellent processability, good tear and impact strength, good stiffness, excellent compatibility with LDPE and LLDPE, excellent drawdown, good moisture barrier properties.

Applications: Multiwall liner, gas flush poultry bags, mailing envelopes, heavy duty shipping sacks, fresh cut produce packaging, coextrusions.

MatWeb has a separate entry for the resin using high stalk extrusion.

This former Total Petrochemicals grade is now a part of the Bayport Polymers joint venture.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.945 g/ccASTM D792
Thickness 25.4 micronsas tested; 2.5 BUR
Melt Flow 0.28 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
High Load Melt Index 20 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 3400 psi
@Thickness 0.0254 mm
ASTM D882A
Film Tensile Strength at Yield, TD 3800 psi
@Thickness 0.0254 mm
ASTM D882A
Film Elongation at Break, MD 450 %
@Thickness 0.0254 mm
ASTM D882A
Film Elongation at Break, TD 600 %
@Thickness 0.0254 mm
ASTM D882A
Elmendorf Tear Strength MD 10 g
@Thickness 0.0254 mm
ASTM D1922
Elmendorf Tear Strength TD 1450 g
@Thickness 0.0254 mm
ASTM D1922
Dart Drop <= 50.0 g/mil
@Thickness 0.0254 mm
ASTM D1709A
Dart Drop Test <= 50.0 g1.0 mil; ASTM D1709A
Film Tensile Strength at Break, MD 9000 psi
@Thickness 0.0254 mm
ASTM D882A
Film Tensile Strength at Break, TD 2700 psi
@Thickness 0.0254 mm
ASTM D882A
1% Secant Modulus, MD 103000 psi
@Thickness 0.0254 mm
ASTM D882A
1% Secant Modulus, TD 145000 psi
@Thickness 0.0254 mm
ASTM D882A
 
Thermal PropertiesOriginal ValueComments
Melting Point 264 °FASTM D3417
 
Processing PropertiesOriginal ValueComments
Melt Temperature 380 - 420 °FExtrusion
 
Descriptive Properties
ProcessFilm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBAYST814 / 221024

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.