MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Petropol Unipren® B3 PRTA010 90A XP14 UP317 TPE-V
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Product Description: 90 Shore A, Elastomer

Resin ID (ISO 1043): TPE-V
Processing: Injection Molding
Color: Black

Information provided by Petropol

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.970 g/cc0.0350 lb/in³ASTM D792
Linear Mold Shrinkage 0.020 - 0.030 cm/cm0.020 - 0.030 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 87 - 9387 - 93ASTM D2240
Tensile Strength at Break >= 12.0 MPa>= 1740 psiASTM D412C
Elongation at Break 511 %511 %ASTM D412C
Modulus of Elasticity  5.20 GPa
@Strain 100 %
754 ksi
@Strain 100 %
ASTM D412C
 6.60 GPa
@Strain 300 %
957 ksi
@Strain 300 %
ASTM D412C
Tear Strength 60.0 kN/m343 pliASTM D624C
 
Processing PropertiesMetricEnglishComments
Processing Temperature 180 - 200 °C356 - 392 °FMolding
Mold Temperature 25.0 - 50.0 °C77.0 - 122 °F
Drying Temperature 80.0 °C176 °F
Dry Time 2.00 hour2.00 hour
 
Descriptive Properties
Under Load Resistance0.4222h 70°C, ASTM D395B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPETROPOL444 / 313352

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.