MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Chesterton Opticool™ 972(E) Synthetic Metalworking Fluid
Categories: Fluid

Material Notes: OPTICOOL 972(E) is a high performance, low maintenance synthetic fluid. It is DEA and Boron free and offers superior lubricity, corrosion inhibition, extreme pressure resistance, rancidity control and hard water stability. OPTICOOL 972(E) is usable in a broad range of machining operations from low to high speed and recommended for alloy steels, cast irons and exotic metals. The heat dissipating properties reduce heat and chip formation, provide rapid cooling of the tool and the workpiece, extending tool life when compared to conventional soluble oils and semi-synthetics.

Properties:

  • Excellent Lubricity
  • Superior Heat Dissipation
  • Synthetic Lubricant Base
  • Extreme Pressure Capability
  • Excellent Hard Water Stability
  • Does Not Mist
  • Oil Intolerant - Reject High % of Tramp Oil
  • Superior Settling Prevents the recalculating of fines
  • Excellent Filterability
  • Resists Microbial Attack
  • Excellent Corrosion Protection.
Suggested uses:
  • Milling
  • Turning
  • Grinding
  • Stamping
  • Drawing
  • Braoching
  • Drilling
  • Reaming
  • Sawing
  • Tapping
  • Fine Threading

Information provided by Chesterton

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.100 g/cc1.100 g/cc
Solubility in Water 100 %100 %
pH 9.29.25% Concentrate
 9.59.5Concentrate
 
Descriptive Properties
AppearanceClear, Yellow5% water
Flash PointNone
FormLiquid Concentrate
Freeze Thaw StabilityPass
Refractometer factor2.0 % per °Brix

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPTCHS107h / 239864

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.