Fibremod™ FE121SF-9502 is a 10% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. This product is stabilized with a halogen-free flame retardant. It has a high tensile strain at break as well as excellent resistance against chemicals and water. It also provides high level of insulation. Applications: Fibremod FE121SF-9502 has been developed for E&E and automotive applications such as the Lithium-Ion battery module housing, cell holder or insulation plate. Special Features: - Flame-Retardant stabilization
- High flowability
- Low density
- Stabilized for contact with metals
- High tensile strain at break
Values determined on standard injection molded specimens conditioned at 23°C and 50% relative humidity after at least 96 hours storage time. To avoid residual humidity from transport or storage, the material should be pre-dried approximately 2h at 80°C.Information provided by Borealis AG |