MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

3M 8087 Construction Seaming Tape
Categories: Polymer; Tape

Material Notes: 3M™ Construction Seaming Tape 8087 is designed to seal seams on housewrap and insulated sheathing products. It can also be used to seam polyethylene vapor barrier products as well as to repair holes and tears in these building materials. Taping seams aids in reducing air infiltration, improving the effectiveness of insulation and reducing heating and cooling costs.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 38.1 microns1.50 milBacking; ASTM D3652
 76.2 microns3.00 milTotal; ASTM D3652
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 46.1 MPa6690 psiASTM D3759
Elongation at Break 130 %130 %ASTM D3759
Peel Strength 0.175 kN/m1.00 pliAdhesion to Polyethylene; ASTM D3330
 0.27391 kN/m1.5625 pliAdhesion to Housewrap; ASTM D3330
 0.49303 kN/m2.8125 pliAdhesion to Steel; ASTM D3330
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 105 °C221 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature >= -10.0 °C>= 14.0 °FApplication
 <= 49.0 °C<= 120 °FApplication
 
Descriptive Properties
Adhesive TypeAcrylic
AppearanceRed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM34450 / 169197

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.