MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ITW Devcon® Silite RTV®
Categories: Polymer; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: A Silicone adhesive/sealant compound for sealing, caulking, bonding, and making gaskets. Uses: Weather-proofing electrical components, caulking plumbing fixtures, sealing glass, and making form-in-place gaskets. Features: Flexible from -60°F to 450°F (white & clear), Moisture curing, Flexible from -60°F to 500°F/ 600°F intermittent (Red), Resistant to weather and chemicals.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.75 lb/galuncured
Viscosity 300000 - 400000 cP
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 30
Tensile Strength 400 psiASTM D412
Elongation at Break 600 %ASTM D412
Tear Strength 47.0 pliASTM D624
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 7.00e+13 ohm-cmASTM D149
Dielectric Constant 2.8ASTM D150
Dielectric Strength 14.8 kV/mmASTM D149
 
Processing PropertiesOriginal ValueComments
Cure Time 168 hour
@Temperature 24.0 °C
As Tested
 
Descriptive Properties
Chemical/Solvent ResistanceAmmonia: fair30 day immersion at 75°F. Sample cured 7 days at RT
 Ammonium Hydroxide 20%: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Cutting oil: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Ethanol: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Gasoline (unleaded): poor30 day immersion at 75°F. Sample cured 7 days at RT
 Glycols/Antifreeze: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Hydrochloric 36%: poor30 day immersion at 75°F. Sample cured 7 days at RT
 Hydrochloric Acid 10%: poor30 day immersion at 75°F. Sample cured 7 days at RT
 Methanol: fair30 day immersion at 75°F. Sample cured 7 days at RT
 Motor Oil: poor30 day immersion at 75°F. Sample cured 7 days at RT
 Nitric 50%l: fair30 day immersion at 75°F. Sample cured 7 days at RT
 Potassium Hydroxide 20%: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Sodium Hydroxide 10%: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Sodium Hydroxide 50%: excellent30 day immersion at 75°F. Sample cured 7 days at RT
 Sodium Hypochlorite: very good30 day immersion at 75°F. Sample cured 7 days at RT
 Sulfuric Acid 10%: very good30 day immersion at 75°F. Sample cured 7 days at RT
Colorclear, white, or red
Coverage100 ft/lb
Tangent Loss1000
ViscosityNon-sag gel up to 3/4".

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PITWD9222 / 239731

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.