MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Polyram Polytron A30B041 Nylon 66, 30% Long Fiber
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: 30% LONG FIBER GLASS REINFORCED, PTFE LUBRICATED, UV STABILIZED BLACK NYLON 6.6 FOR INJECTION MOLDING APPLICATION.

Information provided by Polyram Ram On Ind.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.50 g/ccASTM-D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 170 MPaASTM-D638
Elongation at Break 2.5 %ASTM-D638
Tensile Modulus 9.20 GPaASTM-D790
Flexural Strength 250 MPaASTM-D790
Flexural Modulus 9.25 GPaASTM-D790
Izod Impact, Notched 2.10 J/cm
@Temperature 23.0 °C
ASTM-D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 256 °CDSC
Deflection Temperature at 1.8 MPa (264 psi) 255 °CASTM-D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 205 TFE 15 UV Nylon 6/6 (PA), Glass Fiber - PTFE Lubricated - UV Stabilized
Lehmann & Voss LUVOTECH® GS 58 Polyamide 66 with glass fiber, lubricant modified
Lehmann & Voss LUVOTECH® 1-9513 Polyamide 66 with glass fiber, PTFE, lubricant modified, heat stabilized
Lehmann & Voss LUVOCOM® 1-1129 Polyamide 66 with glass fiber, PTFE, lubricant modified, heat stabilized
Lehmann & Voss LUVOCOM® 1/GF/30/TF/15/HS/BK Polyamide 66 with glass fiber and PTFE, heat stabilized

PPOLYRA385 / 57647

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.