MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Unifrax Isofrax® 1260C Blanket Thermal Insulation
Categories: Ceramic; Oxide; Magnesium Oxide; Silicon Oxide

Material Notes: Isofrax® Thermal Insulation from Unifrax is a fiber that utilizes a unique, patented silica-magnesia chemistry to solve a variety of demanding, high-temperature application problems. Isofrax 1260C Blanket is the product of a long-term research and development effort by Unifrax to produce an insulating blanket which has the high-temperature performance characteristics required in many applications at temperatures up to 2300°F/1260°C and also meets European regulatory requirements (Directive 97/69/EC). Isofrax 1260C Blanket provides low thermal conductivity, excellent thermal stability, thermal shock resistance, low weight, required handling strength, low heat storage, flexibility, and excellent corrosion resistance. Isofrax 1260C Blanket has excellent chemical stability and is unaffected by most chemicals except hydrofluoric and phosphoric acids and concentrated alkalies. If wet by water or steam, thermal and physical properties remain unaffected after drying. Isofrax 1260C Blanket also provides superior resistance to attack from molten aluminum alloys at high temperatures.

    Applications
  • Removable insulating blankets for weld stress relieving
  • Reusable insulation for steam and gas turbines
  • High-temperature kiln and furnace insulation
  • Furnace door linings and seals
  • Furnace repairs
  • Boiler and incinerator linings
  • Seals and gaskets
  • Automotive heat shields
  • Appliance insulation
  • Fire protection
  • Duct, stack and flue linings
  • Vessel covers and lids
  • Personnel heat shields
  • Molten metal splash protection

Information Provided by Unifrax I LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.54 g/cc
Density 6.00 lb/ft³
 8.00 lb/ft³
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 5.00 psiASTM 686-76
 6.00 psiASTM 686-76
 
Thermal PropertiesOriginal ValueComments
Melting Point 1500 °C
Maximum Service Temperature, Air 1260 °CRecommended Operating Temperature
 
Component Elements PropertiesOriginal ValueComments
MgO 18 - 27 %
Other, total 0.00 - 4.0 %Trace Elements
SiO2 70 - 80 %
 
Descriptive Properties
ColorBluish White
Compression Recovery (%)78at 50% Compression
 89at 30% Compression
 96at 10% Compression
Fiber Diameter (microns)3.0 to 5.0
Temperature Grade (°C)1260

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Unifrax Isofrax® 1260C High Index Fiber Thermal Insulation
Chosun Refractories 1260PAPER Paper

CUNIF122 / 97894

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.