MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nouryon Perkadox 16 Polymer Di(4-tert-butylcyclohexyl) peroxydicarbonate
Categories: Other Engineering Material

Material Notes: Initiator for the production of PVC, PVA, PVOH and acrylics.

CAS number: 15520-11-3

EINECS/ELINCS No.: 239-557-1

Applications: Polymer production: Polymerization of vinyl chloride Perkadox 16 is applied as an initiator for the suspension and mass polymerization of vinyl chloride in the temperature range between 40°C and 65°C. Perkadox 16 can be used alone or in combination with other peroxides, such as 1,1,3,3-Tetramethylbutyl peroxyneodecanoate (Trigonox 423), Cumyl peroxyneodecanoate (Trigonox 99) or Dilauroyl peroxide (Laurox), to increase reactor efficiency. For Thermoset: Perkadox 16 is a solid peroxydicarbonate which is used for the curing of unsaturated polyester resins and methacrylic resins mainly in the temperature range of 60°C and higher. Perkadox 16 is not suitable for the production of clear - castings or - coatings, due to a slight haze in the end product. In this case, Perkadox 16S can be advised. Perkadox 16 shows a high reactivity at elevated temperatures, which is demonstrated by its low activation temperature, in combination with a relatively long pot life at ambient temperatures. Perkadox 16 is mostly used in combination with a low reactive peroxide to ensure a good final cure. Combinations of Perkadox 16 with e.g. Trigonox C, Trigonox 29-B50 or Trigonox 21 can therefore successfully be used for those applications where a long gel time or production time is required at room temperature in combination with a fast cure at elevated temperatures of e.g. 60-140°C. Applications area can be: pultrusion, filament winding, manufacturing of artificial marble.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.450 - 0.480 g/cc0.0163 - 0.0173 lb/in³
Density 1.13 g/cc0.0408 lb/in³
Half-life  0.100
@Temperature 82.0 °C
0.100
@Temperature 180 °F
[hr]
 1.00
@Temperature 64.0 °C
1.00
@Temperature 147 °F
[hr]
 10.0
@Temperature 48.0 °C
10.0
@Temperature 118 °F
[hr]
Molecular Weight 398.5 g/mol398.5 g/mol
Storage Temperature <= 20.0 °C<= 68.0 °F
 
Thermal PropertiesMetricEnglishComments
Decomposition Temperature 40.0 °C104 °FSelf-Accelerating Decomposition Temperature
 
Processing PropertiesMetricEnglishComments
Shelf Life 3.00 Month3.00 Month
 
Descriptive Properties
AppearanceWhite powder
Assay94.0-97.0 %
Content= 4000 mg/kgInorganic + organic hydrolysable chloride

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY751 / 286274

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.