0320 exhibits a high melt strength for extrusion processes. The material demonstrates excellent heat and chemical resistance. The intended use of this product is for extruding monofilament/fibers, rod and slab. Available standard in powder (0320B0), pellet (0320P0) and crystallized pellet (0320C0) form.Information provided by Celanese |