SKYPEL P142DF is a thermoplastic polyester elastomer resin superior heat resistance. SKYPEL P142DF with a medium 42D hardness based on shore D scale is widely used for injection molding and extrusion applications. And SKYPEL P142DF is also available to over mold TPU, PC, ABS, PC/ABS alloys. Tensile property tests on ASTM Type IV dumbbells diecut from injection molded slab 2mm thick. Crosshead speed 50 mm/min. Information provided by SK Chemicals |