MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Crucible Steel REX® 95 Tungsten Type High Speed Steel, AISI T8
Categories: Metal; Ferrous Metal; Tool Steel

Material Notes: Rex 95 combines high red hardness, moderate abrasion resistance, and good toughness. This grade is frequently used for more severe cutting applications than M2, such as machining stainless steels. Rex 95 makes an outstanding tool bit for general purpose applications.

Rex AAA is only supplied as tool bits, already heat treated to about HRC 64/66.

Information provided by Crucible Industries

Key Words: AISI T8
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.43 g/ccliterature value
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 64 - 66
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.80 %
Chromium, Cr 4.0 %
Cobalt, Co 5.25 %
Iron, Fe 72.6 %as balance
Manganese, Mn 0.30 %
Molybdenum, Mo 0.75 %
Silicon, Si 0.30 %
Tungsten, W 14 %
Vanadium, V 2.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 1005 Steel
Crucible Steel CPM® REX® M35HCHS High Speed Steel, AISI M35
Carpenter Speed Star® High Speed Steel (Red-Hard) (AISI M2)
Carpenter Four Star High Speed Steel Red-Wear® (AISI M4)
Bohler-Uddeholm BÖHLER S500(m42) High Speed Steel

NCRUC930 / 160381

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.