MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Domo TECHNYL® 1021GF6 PA6, 30% glass fiber, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Description: Polyamide 6, 30% glass fiber reinforced, for injection molding.

Available in: Asia Pacific

Product Applications: TECHNYL® 1021GF6 is used in all sectors of industry, offering an excellent combination between the mechanical properties. This grade is used for It is used in the automotive industry and electrical sectors. Door motor cover. This product is available in Natural, black, gray and in colors on request.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.36 g/ccISO 1183
Water Absorption 0.95 %
@Temperature 23.0 °C,
Time 86400 sec
ISO 62
Linear Mold Shrinkage, Flow 0.0035 cm/cm
Linear Mold Shrinkage, Transverse 0.0065 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 121ASTM D786
Tensile Strength, Yield 175 MPaASTM D638
Elongation at Break 3.5 %ASTM D638
Flexural Strength 260 MPaASTM D790
Flexural Modulus 8900 MPaASTM D790
Izod Impact, Notched 130 J/mASTM D265
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohmIEC 60093
Dissipation Factor 0.020IEC 60250
Comparative Tracking Index 550 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 32.0 µm/m-°C
@Temperature 23.0 - 85.0 °C
ISO 11359
Melting Point 222 °CISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 210 °CASTM D648
Flammability, UL94 HBISO 1210
Glow Wire Flammability Index 650 °C
@Thickness 1.60 mm
IEC-60695-2-12
 
Processing PropertiesOriginal ValueComments
Feed Temperature 230 - 235 °C
Mold Temperature 80.0 - 100 °C
Drying Temperature 80.0 °C
Moisture Content <= 0.20 %
 
Descriptive Properties
Compression Zone235-345°C
Mixing Zone245-250°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo TECHNYL® 1021GF6 PA6, 30% glass fiber, Conditioned
Domo TECHNYL® C 218 V 30 PA6, 30% glass fiber, DRY
Domo TECHNYL® 1015CR PA6, DRY
Covestro Bayblend® FR3000 PC/ABS Blend
Domo TECHNYL® 2411GF6 PA66, 30% glass fiber, DRY

PRHOD564 / 137795

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.