MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

MOL Group TIPELIN FS 340-03 MDPE, Blown films
Categories: Polymer; Thermoplastic; Polyethylene (PE); Medium Density (MDPE); Medium Density Polyethylene (MDPE), Film Grade

Material Notes: Description: TIPELIN FS 340-03 is a film grade of medium density polyethylene copolymer (with hexen-1 as comonomer) that has very good Elmendorf Tear Resistance and excellent Dart Drop Resistance. The grade contains antioxidants and acid scavenger.

Applications: TIPELIN FS 340-03 is recommended for bags, shopping bags, garbage bags, shrink films, multi-layer films and blend component for LDPE. Recommended film thickness is 0.015 to 0.06 mm.

(1) Average mechanical property values of several measurements carried out on standard pressed specimens (ISO 293) conditioned at room temperature (ISO 291). (2) Average mechanical property values of several measurements on film (MD = machine direction, TD = trans direction) thickness of 0.025 mm, blow up ratio 4:1.

Information provided by Molgroup Chemicals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.935 g/cc0.0338 lb/in³1; ISO 1183-1
Oxidative Induction Time (OIT) 25 min
@Temperature 200 °C
25 min
@Temperature 392 °F
EN 728
Melt Flow  0.17 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.17 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133-1
 0.78 g/10 min
@Load 5.00 kg,
Temperature 190 °C
0.78 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ISO 1133-1
 14 g/10 min
@Load 21.6 kg,
Temperature 190 °C
14 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ISO 1133-1
Storage Temperature <= 40.0 °C<= 104 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 60601; ISO 868
Film Tensile Strength at Yield, MD 25.0 MPa3630 psi2; ISO 527-3
Film Tensile Strength at Yield, TD 18.0 MPa2610 psi2; ISO 527-3
Film Elongation at Break, MD 700 %700 %2; ISO 527-3
Film Elongation at Break, TD 800 %800 %2; ISO 527-3
Flexural Modulus 0.800 GPa116 ksi1; ISO 178
Impact 37372, Spencer; ASTM D 3420
Elmendorf Tear Strength MD 50 g50 g2; ISO 6383-2
Elmendorf Tear Strength TD 336 g336 g2; ISO 6383-2
Dart Drop Test 86.0 g0.190 lb2, F50; ISO 7765-1 method A
Film Tensile Strength at Break, MD 51.0 MPa7400 psi2; ISO 527-3
Film Tensile Strength at Break, TD 43.0 MPa6240 psi2; ISO 527-3
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 118 °C244 °F1; ISO 306/A 120
 
Processing PropertiesMetricEnglishComments
Processing Temperature 180 - 220 °C356 - 428 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMOLG028 / 297194

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.