MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ZEON Nipol® 1022 Nitrile Elastomer
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Nipol 1022 is a copolymer of butadiene and acrylonitrile with medium oil resistance and is directly soluble in many solvents without the necessity of mill breakdown. Sufficient nonstaining antioxidant has been added during manufacture for normal storage conditions.

Low viscosity, directly soluble with wide FDA acceptance.

Key Words: NBR
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.980 g/cc
Viscosity 1000 - 4200 cPUnmilled Cement; Zeon Test #328
Mooney Viscosity 40 - 55
@Temperature 100 °C
(1+4)
Ash <= 1.0 %Zeon Test #873
 
Descriptive Properties
AO TypeNS
Bound ACN (%, acrylonitrile)32-34
Heat Loss (%) Max1
Hot/ColdH

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ZEON Nipol® DN3350 Nitrile Elastomer
ZEON Nipol® 1072 Carboxylated Nitrile Elastomer
ZEON Nipol® 1072CGX Carboxylated Nitrile Elastomer
Dow Nucrel® 699 Ethylene-Methacrylic Acid Copolymer Resin
ZEON Zealloy® 1422 Modifier for Thermoplastics

PZEONB39 / 72998

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.