MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro DESMOPHEN® 1300 BA Polyurethane
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Characterization: Polyester polyol. As the co-reactant for polyisocyanates in the formulation of air-drying, two-pack coatings.

Properties / Applications: Desmophen® 1300 BA is especially suitable for the formulation of fast-drying, two-pack coatings. They are mainly used for clear and pigmented finishes for wood, chipboard and hardboard.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.06 g/cc1.06 g/ccDIN EN ISO 2811-2
Volatiles 24 - 26 %24 - 26 %2 g resin/2 ml toluene/1 h at 125 °C, convection oven; DIN EN ISO 3251
Viscosity 800 - 1200 cP800 - 1200 cPDIN EN ISO 3219/A.3
 
Chemical PropertiesMetricEnglishComments
Acid Value 6.0 - 126.0 - 12[mg KOH/g]; DIN EN ISO 2114
 
Thermal PropertiesMetricEnglishComments
Flash Point 30.0 °C86.0 °FDIN EN ISO 1523
 
Processing PropertiesMetricEnglishComments
Moisture Content >= 0.10 %>= 0.10 %DIN 51 777/1
 
Descriptive Properties
Color<4Iodine, DIN EN 1557
Content2.9-3.5%Hydroxyl, DIN 53 240/2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro DESMOPHEN® 651 MPA Polyurethane
Covestro DESMOPHEN® 650A-65 PMA Polyurethane
Covestro DESMOPHEN® 650 MPA Polyurethane
Covestro DESMOPHEN® 631 MPA Polyurethane
Plywood

PCOVEST0740 / 202523

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.