MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Morgan Advanced Ceramics Insulite LR Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Calcined Fireclay/Perlite raw material base. Hydraulic bond. A versatile 1370°C insulating gunning material with low thermal conductivity and excellent adhesion properties without the need for pre-dampening.

Applications: General purpose insulating gunning grade which can be used for hot face or back up insulation.

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 1.48 g/cc0.0535 lb/in³dried to 110°C
Grain Size <= 6000 µm<= 6000 µm
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength  2.00 MPa
@Treatment Temp. 815 °C
290 psi
@Treatment Temp. 1500 °F
Cold Crushing Strength
 4.00 MPa
@Treatment Temp. 110 °C
580 psi
@Treatment Temp. 230 °F
Cold Crushing Strength
 12.0 MPa
@Treatment Temp. 1370 °C
1740 psi
@Treatment Temp. 2500 °F
Cold Crushing Strength
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.330 W/m-K
@Temperature 200 °C
2.29 BTU-in/hr-ft²-°F
@Temperature 392 °F
 0.350 W/m-K
@Temperature 400 °C
2.43 BTU-in/hr-ft²-°F
@Temperature 752 °F
 0.370 W/m-K
@Temperature 600 °C
2.57 BTU-in/hr-ft²-°F
@Temperature 1110 °F
 0.390 W/m-K
@Temperature 800 °C
2.71 BTU-in/hr-ft²-°F
@Temperature 1470 °F
 0.410 W/m-K
@Temperature 1000 °C
2.85 BTU-in/hr-ft²-°F
@Temperature 1830 °F
 0.430 W/m-K
@Temperature 1200 °C
2.98 BTU-in/hr-ft²-°F
@Temperature 2190 °F
Maximum Service Temperature, Air <= 1370 °C<= 2500 °F
Shrinkage  0.00 - 0.20 %
@Treatment Temp. 110 °C
0.00 - 0.20 %
@Treatment Temp. 230 °F
 0.60 %
@Treatment Temp. 1100 °C
0.60 %
@Treatment Temp. 2010 °F
 2.0 %
@Treatment Temp. 1370 °C
2.0 %
@Treatment Temp. 2500 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 35 %35 %
CaO 10 %10 %
Fe2O3 6.5 %6.5 %
K2O+Na2O 1.5 %1.5 %Na2O + K2O
MgO 0.70 %0.70 %
SiO2 43 %43 %
TiO2 1.8 %1.8 %
 
Descriptive Properties
Net Material Required (kg/m³)1380
Water Additionadded at nozzle, 25 kg bag weight.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CMORF6369 / 203153

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.