MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polytek Poly-Fast 72-40 Flexible, Polyurethane Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Description: Poly-Fast 72-40 Liquid Rubber consists of two parts (A and B) that, after mixing in the correct ratio, cure at room temperature to a versatile mold rubber. This liquid rubber may be poured or thickened and applied by trowel or brush, to make tough, flexible molds. These molds are useful for casting wax or plaster.

Product Line Features:

  • For sculptural applications and investment casting with wax
  • Pour or brush-on with the addition of a liquid thickener
  • Vary hardness with the addition of softener
  • Good flow and bubble release resulting in reproduction of the finest details
  • For long library life from cured molds, consider Poly 74-Series rubbers

Information provided by Polytek

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 4000 cP4000 cPMixed
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4040
 
Processing PropertiesMetricEnglishComments
Cure Time 30.0 min0.500 hourPour Time
 
Descriptive Properties
Cured ColorIvory
Mix Ratio By Weight1A:10B
Specific Volume20 in3/lb

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPTK5062 / 251054

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.