MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Röchling Glastic Laminates/Shapes SG-200 High Strength/High Temperature Polyester Laminate
Categories: Polymer; Thermoset; Composite SMC; Polyester, TS

Material Notes: Data provided by Glastic Corporation.

NEMA GPO-1. A superior replacement for epoxy-bonded mica in layer insulation applications.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.70 g/ccASTM D792
Water Absorption 0.30 %ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 86.0 MPaASTM D638
Tensile Modulus 12.0 GPaASTM D638
Flexural Yield Strength 200 MPaASTM D790
Compressive Yield Strength 248 MPaASTM D695
Shear Strength 77.0 MPaASTM D732
Izod Impact, Notched 6.40 J/cmASTM D256
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 1.45e+14 ohmInsulation Resistance, ASTM D257
Dielectric Constant 3.7
@Frequency 1e+6 Hz
ASTM D150
 4.6
@Frequency 60 Hz
ASTM D150
Dielectric Strength 20.0 kV/mmPerpendicular, Short-term, in air; ASTM D149
Dissipation Factor 0.013
@Frequency 1e+6 Hz
ASTM D150
 0.037
@Frequency 60 Hz
ASTM D150
Arc Resistance 180 secPost-cured, ASTM D495
Comparative Tracking Index >= 500 VUL746A
Hot Wire Ignition, HWI 39 sec0.058 in, UL746A
High Amp Arc Ignition, HAI 200 arcsUL746A
High Voltage Arc-Tracking Rate, HVTR 0.000 mm/minUL746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear 20.0 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Thermal Conductivity 0.240 W/m-KASTM C177
Maximum Service Temperature, Air 200 °CNEMA temperature
UL RTI, Electrical 210 °CUL 746B
UL RTI, Mechanical with Impact 210 °CUL 746B
Flammability, UL94 HB
Oxygen Index 21.8 %ASTM D2862

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Röchling Glastic® SG-200 Polyester Laminate
AISI 1010 Steel, cold drawn
AISI 1020 Steel, annealed at 870°C (1600°F)
A. Schulman Premi-Glas® 2206-15 CR-SX Fiberglass Reinforced Thermoset SMC
34MoCr4 Alloy Steel

PGLASE / 41915

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.