40 Shore D, Slightly Lubricated, High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow MoldingWhile this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product. |