MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chosun Refractories A65 Special High-Density Gunning Castable
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes:

Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density  2.66 g/cc
@Temperature 1000 °C,
Time 10800 sec
0.0961 lb/in³
@Temperature 1830 °F,
Time 3.00 hour
 2.66 g/cc
@Temperature 1500 °C,
Time 10800 sec
0.0961 lb/in³
@Temperature 2730 °F,
Time 3.00 hour
 2.69 g/cc
@Temperature 110 °C,
Time 86400 sec
0.0972 lb/in³
@Temperature 230 °F,
Time 24.0 hour
Porosity  19.5 %
@Temperature 110 °C,
Time 86400 sec
19.5 %
@Temperature 230 °F,
Time 24.0 hour
 24 %
@Temperature 1500 °C,
Time 10800 sec
24 %
@Temperature 2730 °F,
Time 3.00 hour
 24.5 %
@Temperature 1000 °C,
Time 10800 sec
24.5 %
@Temperature 1830 °F,
Time 3.00 hour
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture  0.0034335 GPa
@Temperature 110 °C,
Time 86400 sec
0.49799 ksi
@Temperature 230 °F,
Time 24.0 hour
 0.003924 GPa
@Temperature 1000 °C,
Time 10800 sec
0.5691 ksi
@Temperature 1830 °F,
Time 3.00 hour
 0.003924 GPa
@Temperature 1500 °C,
Time 10800 sec
0.5691 ksi
@Temperature 2730 °F,
Time 3.00 hour
 
Thermal PropertiesMetricEnglishComments
Shrinkage  -0.0600 %
@Temperature 110 °C,
Time 86400 sec
-0.0600 %
@Temperature 230 °F,
Time 24.0 hour
 -0.0600 %
@Temperature 1000 °C,
Time 10800 sec
-0.0600 %
@Temperature 1830 °F,
Time 3.00 hour
 0.050 %
@Temperature 1500 °C,
Time 10800 sec
0.050 %
@Temperature 2730 °F,
Time 3.00 hour
 
Component Elements PropertiesMetricEnglishComments
Al2O3 65 %65 %
SiC 30 %30 %
SiO2 1.0 %1.0 %
 
Descriptive Properties
Main ApplicationsBlast furnace Main runner
Material Required for Estimating (kg/m3)2,700

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CCHOS233 / 124177

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.