MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Röchling EtroX® CM Machinable Polymer
Categories: Polymer; Thermoplastic

Material Notes: EtroX® I CM is a polyimide polymer designed to meet the demanding requirements of the electronics, aerospace, and automotive industries. It maintains high performance under extreme conditions due to its high-temperature resistance and mechanical strength at elevated temperatures. The material offers high tensile strength and dimensional stability, ensuring reliability in demanding applications with strong mechanical properties.

EtroX® I CM can withstand temperatures exceeding 250°C / 482°F, making it suitable for replacing metals in high-heat environments. Its low inherent flammability is crucial for applications where safety is a priority. It can be precision machined using conventional CNC machines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.37 g/ccDIN EN ISO 1183-1
Water Absorption 0.150 %Immersion, 24 hrs.; DIN EN ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 89DIN EN ISO 868
Tensile Strength 2.03 ksiASTM D638
Elongation at Break 14.2 %ASTM D638
Tensile Modulus 500000 psiASTM D638
Flexural Strength 24.0 ksiASTM D790
Flexural Modulus 561 ksiASTM D790
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 1e+15 ohmDIN EN 62631-3-2
Dielectric Constant 3.3
@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 864 V/milIEC 60243-1
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 260 °C
Deflection Temperature at 1.8 MPa (264 psi) 319 °CDIN EN ISO 75-1/-2
Minimum Service Temperature, Air -195 °C
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PROCH9067c / 326948

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.