MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Teknor Apex Chemlon® 66A Nylon 66, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: Notes: 66A is general purpose unfilled injection molding grade of nylon 66.

Availability: Europe

Features: General Purpose

Uses: General Purpose

Form: Pellets

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 - 1.15 g/cc0.0408 - 0.0415 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.014 - 0.019 cm/cm0.014 - 0.019 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 55.0 MPa7980 psiISO 527-2
Tensile Modulus 1.70 GPa247 ksiISO 527-2
Flexural Strength 20.0 MPa2900 psiISO 178
Flexural Modulus 0.752 GPa109 ksiISO 178
Izod Impact, Notched (ISO) 9.03 kJ/m²4.30 ft-lb/in²ISO 180
Izod Impact, Unnotched (ISO) NBNBISO 180
Charpy Impact Unnotched NBNBISO 179
Charpy Impact, Notched NBNBISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+12 ohm1.00e+12 ohmIEC 60093
Dielectric Strength 11.0 kV/mm
@Thickness 3.00 mm
280 kV/in
@Thickness 0.118 in
IEC 60243-1
Dissipation Factor 0.040
@Frequency 1e+6 Hz
0.040
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index >= 600 V>= 600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 175 °C347 °FUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C140 °FUnannealed; ISO 75-2/A
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 270 - 290 °C518 - 554 °F
Middle Barrel Temperature 270 - 290 °C518 - 554 °F
Front Barrel Temperature 270 - 290 °C518 - 554 °F
Melt Temperature <= 300 °C<= 572 °F
Mold Temperature 80.0 - 90.0 °C176 - 194 °F
Drying Temperature 80.0 °C176 °F
Dry Time 2.00 hour2.00 hour
Screw Speed >= 50 rpm>= 50 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ0401 / 236892

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.