MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Precision Polymer Engineering E80E Ethylene Propylene Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: General Purpose, Ethylene Propylene Terpolymer (EPT) 75-85 IRHD. Terpolymer of ethylene, propylene and diene monomers. To meet Aerospace specification DTD 5597A Grade 80. ASTM & ISO designation = EPDM.

Applications: For sealing applications where good fluid resistance and low compression set are of prime importance. For continuous and/or intermittent use in contact with phosphate ester or silicone hydraulic fluids within the temperature ranges as quoted. Suitable for applications in contact with air, this material has excellent resistance to ozone. Unsuitable for use in contact with fuels, mineral oil based and diester oils and silicate fluids or greases derived from these.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80°IRHD; ASTM D1415
 90°IRHD, +10 change after 168 hours @ 125°C; ASTM D1415
Tensile Strength, Yield 9.775 MPa-15% change after 168 hours @ 125°C; ASTM D412
 11.5 MPaASTM D412
Elongation at Break 136 %-20% change after 168 hours @ 125°C; ASTM D412
 170 %ASTM D412
Compression Set 20 %
@Temperature 100 °C,
Time 86400 sec
ASTM D395
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 160 °C
Minimum Service Temperature, Air -60.0 °C
 -40.0 °CTemperature at which rigidity modulus shall not exceed 70 Mpa
Flash Point >= 200 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Precision Polymer Engineering E60Q Ethylene Propylene Rubber
Precision Polymer Engineering E63B Ethylene Propylene Rubber
Precision Polymer Engineering E70A Ethylene Propylene Rubber
Precision Polymer Engineering E70H Ethylene Propylene Rubber
Precision Polymer Engineering E70K Ethylene Propylene Rubber

PPRECI067 / 57791

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.