MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Daikin DAI-EL LATEX GL-252EA Water-based Fluoroelastomer Coating
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer

Material Notes: Water-based fluoroelastomer coating for elasticity and heat resistance.

Introduction: DAI-EL LATEX GL grade is a water-based fluoroelastomer coating; GL-200RB is mixed to cure the layer before applying; DAI-EL LATEX GL-252EA makes a black coating layer displaying elasticity and heat resistance; It is good for surface modification of elastic substrate

Information provided by Daikin.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 51.0 %51.0 %
pH 7.607.60
Viscosity 100 cP100 cP
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 7.60 MPa1100 psi
Elongation at Break 170 %170 %
100% Modulus 5.60 MPa
@Strain 100 %
812 psi
@Strain 100 %
 
Processing PropertiesMetricEnglishComments
Sintering Temperature 120 - 250 °C248 - 482 °F
 
Descriptive Properties
AppearanceBlack Film
International Rubber Hardness Degree73
n-Hexadecane Contact Angle (°)49°
Water Contact Angle (°)91°

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDAIK9685 / 327125

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.