MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Capron® 8233G 33% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Capron 8233G is a 33% glass fiber reinforced polyamide 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. It is also available in heat stabilized (Capron 8233G HS) and/or pigmented versions.

Capron 8233G is generally recommended for applications such as power tool housings, weed trimmer components, gears, automotive housings and under hood applications.

Data provided by Allied Signal.

Processing: Max. water content 0.12%. Product is supplied in sealed containers and drying is not required. If drying becomes necessary, a dehumidifying or desiccant dryer operating at 85°C (185 °F). Is recommended. Drying time is dependent on moisture level.

Melt Temperature: 270-295 degC (518-563 degF). Mold Temperature: 80-95 degC (176-203 degF). Injection and Packing Pressure: 35-125 bar (500-1500psi) This product can be processed over a wide range of mold temperatures; however, for applications where aesthetics critical, a mold surface temperature of 80-95 degC (176-203 degF) is required. Injection pressure controls the filling of the part and should be applied for 90% of ram travel. Packing pressure affects the final part and can be used effectively in controlling sink marks and shrinkage. It should be applied and maintained until the gate area is completely frozen off. Back pressure can be utilized to provide uniform melt consistency and reduce trapped air and gas. A maximum of 3.5 bar (50 psi) is recommended to minimize glass fiber breakage. Fast fill rates are recommended to insure uniform melt delivery to the cavity and prevent premature freezing. Surface appearance is directly affected by injection rate.

Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.38 g/ccISO data
Water Absorption 1.1 %24 hrs; ISO data
Moisture Absorption at Equilibrium 1.8 %50% RH; 23°C; ISO data
Water Absorption at Saturation 6.4 %in water; 23°C; ISO data
Viscosity Measurement 50Formic Acid Viscosity; ISO data
Linear Mold Shrinkage 0.0020 cm/cmISO data
 0.0030 cm/cmASTM data MD
Linear Mold Shrinkage, Transverse 0.0090 cm/cmISO Data
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 195 MPaSame value from ASTM and ISO tests; 5 mm/min.
Elongation at Break 3.5 %ASTM, 5 mm/min
 3.5 %ISO, 5 mm/min
Tensile Modulus 10.3 GPasame value from ASTM and ISO test.
Flexural Yield Strength 300 MPaASTM Data
Flexural Modulus 8.20 GPaISO Value
 9.035 GPaASTM Value
Poissons Ratio 0.35ISO data
Shear Modulus 3.80 GPacalculated
Charpy Impact, Notched 1.40 J/cm²ISO Data
 1.10 J/cm²
@Temperature -30.0 °C
ISO data
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity >= 1.00e+15 ohm-cmISO data
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 21.0 µm/m-°C
@Temperature 20.0 °C
ISO data
CTE, linear, Transverse to Flow 70.0 µm/m-°C
@Temperature 20.0 °C
ISO data
Melting Point 220 °CASTM and ISO test
Deflection Temperature at 0.46 MPa (66 psi) 218 °CValue for both ASTM and ISO data.
Deflection Temperature at 1.8 MPa (264 psi) 207 °CISO data
 210 °CASTM Data
Flammability, UL94 HB
@Thickness 0.710 mm
 HB
@Thickness 3.00 mm
 
Processing PropertiesOriginal ValueComments
Drying Temperature 85.0 °CSee Materials Notes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® 8233G HS 33% Glass Filled PA6 (Conditioned)
BASF Ultramid® 8233G HS 33% Glass Filled PA6 (Dry)
BASF Capron® 8233G 33% Glass-Filled Nylon 6 (Conditioned)
DuPont Mobility and Materials Zytel® 8018HS NC010 PA66-IGF14
BASF Ultramid® 8233G HS BK-102 33% Glass Filled PA6 (Dry)

PALC57 / 23851

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.