MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Total ESD 201 B HDPE blow molding
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: FINATHENE® ESD 201 B is a black conductive compound manufactured from high performance Finathene high density polyethylene. The use of this HDPE compound gives outstanding compatibility to (semi) high molecular weight, high density polyethylene and assures smooth processing on typical machines used in the industry.

FINATHENE® ESD 201B has been developed for the production of high performance industrial parts, intended for use in explosive/hazardous atmospheres.

Information provided provided by Total Petrochemicals.

Total Petrochemicals acquired former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.995 g/ccISO 1183
Environmental Stress Crack Resistance >= 250 hourASTM D1693-70
Melt Flow 4.5 g/10 min
@Temperature 190 °C
High Load; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Flexural Modulus 1.20 GPaISO 178
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 10000 ohm-cm
Surface Resistance <= 10000 ohm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Paxon™ AS55-003 Blow Molding Resin
Overview of materials for Polypropylene, Blow Molding Grade
ExxonMobil Paxon™ BA50-120 High Density Polyethylene Resin
ExxonMobil Paxon™ BA50-100 Blow Molding Resin
ExxonMobil Paxon™ AF50-003 Blow Molding Resin

PFINAP068 / 38651

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.