MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Goodfellow Tin 60/Lead 39/Antimony 1 Alloy
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy; Tin Alloy

Material Notes: A general purpose, low melting point soft solder which can also be used as a protective coating and for metal film capacitors.

Information provided by Goodfellow.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.42 g/cc0.304 lb/in³
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000148 ohm-cm0.0000148 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 24.0 µm/m-°C
@Temperature 15.0 - 110 °C
13.3 µin/in-°F
@Temperature 59.0 - 230 °F
Thermal Conductivity 50.2 W/m-K348 BTU-in/hr-ft²-°F
Melting Point 183 °C361 °F
 
Component Elements PropertiesMetricEnglishComments
Antimony, Sb 1.0 %1.0 %
Lead, Pb 39 %39 %
Tin, Sn 60 %60 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Johnson Matthey 95A Lead-Free Soft Solder Alloy
Johnson Matthey JM 97C Soft Solder/Flux
Johnson Matthey JM 99C Soft Solder/Flux
Johnson Matthey JM P35 Soft Solder/Flux
Johnson Matthey JM P40 Soft Solder/Flux

NGOODF228 / 16285

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.