MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Eastman PG400 PET  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Unreinforced

Material Notes: Voridian PET PG400 is a general purpose resin is mostly supplied into Mexico and has a wide array of applications in container manufacturing.

Applications/Uses

  • Beverage packaging
  • Containers
  • Food packaging
  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Bulk Density 0.817 g/cc0.0295 lb/in³ASTM D1895
    Density 1.40 g/cc0.0506 lb/in³Crystalline Density; ASTM D1505
    Melt Density 1.20 g/cc
    @Temperature 285 °C
    0.0434 lb/in³
    @Temperature 545 °F
    ASTM D1238
    Particle Size 2500 µm2500 µmPellet Size
    Viscosity Measurement 0.78 - 0.820.78 - 0.82Intrinsic; EMN-A-AC-G-V-1
     
    Thermal PropertiesMetricEnglishComments
    Melting Point 240 °C464 °FCrystalline Peak; ASTM D3418
     
    Descriptive Properties
    Acetaldehyde<3ppmVKCA-A-AS-G-GC-0001
    Color, CIE a*-2.5 ± 1.5VGAS-A-AN-G-RS-001
    Color, CIE b*0.3 ± 1.5VGAS-A-AN-G-RS-001
    Color, CIE L*77.5 minVGAS-A-AN-G-RS-001
    Fines, wt%, max0.05VGAS-A-AN-G-GA-1
    Pellet ShapeCubical

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    ExxonMobil Exceed™ PP9122 Polypropylene Homopolymer
    ExxonMobil Exceed™ 1012HA Metallocene Polyethylene Resin
    Envalior Stanyl® TC551 PA46 FR(17)
    Envalior Arnitel® PL380 TPC-ET, Injection Molding
    Envalior Arnitel® EM400 TPC-ET, Injection Molding or Extrusion Grade

    PE9148 / 35205

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.