MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
CRP Technology Windform® GF 2.0 Polyamide-Aluminum-Glass Composite
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: Processed by selective laser sintering (SLS). Windform® GF 2.0 is the evolutionary substitute for Windform GF, our first generation material. Windform® GF 2.0 is a composite material made of polyamide filled with glass and aluminium, which presents an improvement in both the thermal and mechanical properties, and the aesthetics of the product. In terms of performance, Windform® GF 2.0 shows a significant improvement in the HDT (almost +8%), that is, the heat deflection temperature as well as an increase in the values of tensile strength and elongation strength, therefore offering greater ductility than the previous version,

Example Applications: Objects of design and functional aesthetic reproduction, intake manifolds (intake and cooling ducts, air inlet systems), hydraulic ducts (fluid temperature further elevated up to 134°C), fuel systems and household appliances.

Information provided by CRP Technology.

Vendors:   About CRP Technology
CRP Technology (Modena, Italy) develops, manufactures and sells its proprietary high performance composite materials Windform® for professional 3D Printing. It is also distinguished by its know-how in Selective Laser Sintering technology. It offers part production for short- and low-run production, and prototyping services with Windform®. Its specific application fields including but are not limited to: automotive and motorsports, design, aerospace, UAVs, marine, entertainment, defense, and packaging.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.41 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 50.6 MPaUNI EN ISO 527-1(97) and UNI EN ISO 527-2(97)
Elongation at Break 4.6 %UNI EN ISO 527-1(97) and UNI EN ISO 527-2(97)
Tensile Modulus 4.304 GPaUNI EN ISO 527-1(97) and UNI EN ISO 527-2(97)
Flexural Strength 80.2 MPaUNI EN ISO 14125: 2000
Flexural Modulus 3.43 GPaUNI EN ISO 14125: 2000
Charpy Impact Unnotched 2.185 J/cm²ISO 179-1:2007
Charpy Impact, Notched 0.472 J/cm²ISO 179-1:2007
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1e+13 ohm-cmASTM D257-93
Surface Resistance 9.1e+13 ohmASTM D257-93
 
Thermal PropertiesOriginal ValueComments
Melting Point 179.6 °CISO 11357-2
Deflection Temperature at 1.8 MPa (264 psi) 134.3 °CASTM D648
Vicat Softening Point 168.7 °C10 N; ASTM D1252
 
Descriptive Properties
ColorAluminum
Specific Flexural Modulus2432.62[MPa/(g/cc)], Flexural Modulus per density unit
Specific Flexural Strength56.88[MPa/(g/cc)], Flexural Strength per density unit
Specific Tensile Modulus3052.48[MPa/(g/cc)], Tensile Modulus per density unit
Specific Tensile Strength35.89[MPa/(g/cc)], UTS per density unit
Surface Finish1.8 Ra µmAfter Finishing
 6.0 Ra µmAfter SLS Process

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CRP Technology Windform® SP Polyamide-Carbon Fiber Composite for 3D Printing
CRP Technology Windform® XT 2.0 Polyamide-Carbon Fiber Composite
3D Systems DuraForm® PA Nylon for SLS® Systems
3D Systems DuraForm® GF Glass Filled Nylon
ALM PA 650 Nylon 12 SLS Prototyping Polymer

PCRPT00b / 130416

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.