MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Process Technologies Inc Sanifluor® 1000 Formulated Aflas® Elastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: O-Rings, Gaskets and Seals produced from Sanifluor® 1000 have excellent chemical, heat and steam resistance. They provide superior performance in hot water, steam and virtually all caustics; making them ideal for pharmaceutical, medical, biotechnology, food, beverage and cosmetic manufacturers who use steam or caustic chemicals or a combination of both in their sterilization processes. These very aggressive conditions can be too harsh for commonly used sealing materials such as Silicone, EPDM and FKM. Sanifluor® provides excellent performance in SIP (steam in place), CIP (clean in place) and WFI (water for injection) applications. Sanifluor® 1000 is formulated for use in gaskets and seals where both USP and FDA compliance is required.** It also complies with 3-A Sanitary Standard for multiple-use rubber materials. Sanifluor® 1000 meets the extractive requirements of FDA 21CFR177.2600.

Information provided by Process Technologies Inc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.65 g/ccASTM D297
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80ASTM D2240
Tensile Strength at Break 2600 psiASTM D1412
Elongation at Break 170 %ASTM D1414
50% Modulus 0.845 ksi
@Strain 50 %
ASTM D1414
100% Modulus 1.71 ksi
@Strain 100 %
ASTM D1414
Compression Set 30 %
@Temperature 200 °C,
Time 252000 sec
25% Deflection, in Air % of original deflection; ASTM D395
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 230 °C
Minimum Service Temperature, Air -5.00 °C
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
ColorBlack
Compatibility for ChemicalsAcetoneNot Recommended
 AmmoniaNot Recommended
 Hydrochloric AcidExcellent
 Hydrofluoric AcidGood
 Hydrogen PeroxideExcellent
 Isopropyl AlcoholExcellent
 Nitric AcidGood
 Phosphoric AcidExcellent
 Sodium HydroxideExcellent
 Sodium HypochloriteExcellent
 Steam to 400ºF (204ºC)Excellent
 Sulfuric AcidExcellent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Precision Polymer Engineering E80Q Ethylene Propylene Rubber
Trelleborg E849 EPDM Rubber
Greene Tweed FLUORAZ® 890 Fluoroelastomer, FEPM
Process Technologies Inc Viton® Extreme™ Compound 2001 Sanitary Gasket/O-Ring
Process Technologies Inc Tyfluor™ 1000 Sanitary Gasket

PPTI01 / 138113

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.