MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Röchling Trafobard® HD-PH High performance insulation
Categories: Polymer; Thermoset

Material Notes: Components for oil filled power transformers

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.15 - 1.35 g/ccIEC 60763-2
Oil Absorption 10 %IEC 60763-2
Moisture Absorption <= 5.00 %IEC 60763-2
pH 6.5IEC60763-2
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity 10.5 GPaPerpendicular, CMD; DIN EN ISO 178
 13.0 GPaPerpendicular, MD; DIN EN ISO 178
Flexural Strength 110 MPaPerpendicular, CMD; DIN EN ISO 178
 120 MPaPerpendicular, MD; DIN EN ISO 178
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength >= 9.00 kV/mmIN OIL; IEC 243-1
 
Thermal PropertiesOriginal ValueComments
Shrinkage, MD 0.20 %IEC 60763-2
 0.30 %CMD; IEC 60763-2
 
Descriptive Properties
Compressibility (%)2.6IEC 60763-2
 93Reversible part of compressibility, IEC 60763-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Manganese (II, III) Oxide, Mn3O4 (Hausmannite)
Magnesium Fluoride, MgF2 (Sellaite)
Iron (III) Oxide, Fe2O3 (Maghemite)
Harris Acoustic Sensors EC-98 Lead Magnesium Niobate Piezoelectric
Ferroxdur® Hard Magnetic Material

PROCH9118 / 232821

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.