MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Solvay DURATOOL® 450 BMI Tooling Prepreg
Categories: Polymer; Thermoset; Bismaleimide (BMI)

Material Notes: Description: DURATOOL 450 is a proven, high-performance bismaleimide (BMI) resin/carbon fiber tooling system that is capable of continuous service at 375°F (190°C) and short cycle service at 400°F (204°C). DURATOOL 450 allows high-quality tooling laminates to be produced directly from a high-temperature master models or a variety of intermediate materials. After autoclave processing for the initial cure, the tool laminate can be de-molded and post-cured “free-standing”. DURATOOL 450 is supplied in roll form with a standard roll length of 50 yards (50 meters). Standard material width is 50 inches (1000 – 1250mm). Materials are shipped frozen and in insulated boxes.

Features & Benefits:

  • Proven capable of more than 1000 autoclave cycles at 375°F (190°C) without deterioration
  • Manufactured to ensure uniform resin distribution in fabrics with <1% volatile content
  • Formulated for long term thermal oxidative stability during normal 375°F (190°C) service
  • Exhibits low and predictable shrinkage allowing manufacturing process design to net size tool
  • Closely matches the thermal expansion coefficient of composite parts reducing dimensional inaccuracies and residual stress levels
  • Determined safe to use via extensive toxicological screening (contains no MDA or VCHDs)
Suggested Applications:
  • Ideal for multiple-tool/high-production-rate manufacture of composite components

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 1.0 %
 
Thermal PropertiesOriginal ValueComments
CTE, linear 2.50 µm/m-°C
Maximum Service Temperature, Air 190 °Clong-term
Glass Transition Temp, Tg 296 °C
Shrinkage 0.030 %
 
Processing PropertiesOriginal ValueComments
Gel Time 10.0 min
@Temperature 177 °C
Shelf Life 24.0 Month
@Temperature -18.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Henkel Hysol EA 9673 (BMI) Film Adhesive
Hexcel® HexPly® F650 Bismaleimide Resin
Hexcel® HexTOOL™ M61 Quasi-isotropic High Temperature Prepreg Tooling Compound
HOS-Technik Homide 250 Bismaleimide Resin
Solvay FM® 475 BMI Syntactic Core

PCYTED192 / 180494

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.