MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lanxess LEWATIT® GF 202 Cation Exchange Resin
Categories: Polymer; Thermoset

Material Notes: Lewatit® GF 202 is a macroporous cation exchange resin with beads of uniform particle size. The monodispersity imparts excellent kinetics to this mechanically and chemically very robust resin. It has been developed for the removal of glycerin and soaps from biodiesel in fixed beds. After simple preconditioning with 2 BV of methanol it is ready for use. Preconditioning with methanol has the purpose to strip water from the resin. Features of this res are:
  • High glycerin capacities (at a throughput of 1 to 2 BV/h up to 250 g/l)
  • Simultaneous removal of soaps and salts
  • low pressure drop across the bed (40-50 kPas)
Benefits of the biodiesel purification based on ion exchange technology instead of the conventional purification by washing with water are:
  • No waste water
  • Robust and low-cost process
  • Regenerant methanol is simply recycled to the transesterification stage

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.740 g/cc
Density 1.24 g/cc
Bead Size 0.600 - 0.700 mmMean
Storage Temperature -20.0 - 40.0 °C
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 50.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Descriptive Properties
AppearanceOpaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLANY8745 / 209138

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.