MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ineos H05A-00 Polypropylene Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Grade H05A-00 is an antistatic polypropylene homopolymer for injection molding & extrusion applications. This material meeets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520 and is Drug Master file listed.Suggested fabrication methods: Injection molding; Extrusion

Features: Antistatic

Typical applications: Closures, Tubing

Complies with FDA specification, Title 21, CFR 177.1520.

Typical property data below from injection molded samples.

Key Words: Antistatic
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.913 g/cc0.0330 lb/in³ASTM D792
Water Absorption <= 0.010 %<= 0.010 %24 hours; ASTM D570
Linear Mold Shrinkage 0.010 - 0.025 cm/cm0.010 - 0.025 in/inASTM D955
Melt Flow 5.1 g/10 min
@Load 2.16 kg,
Temperature 230 °C
5.1 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 103103Injection Molded; ASTM D785
Tensile Strength at Break 18.0 MPa2610 psi2.0 in/min, Injection Molded; ASTM D638
Tensile Strength, Yield 36.9 MPa5350 psi2.0 in/min, Injection Molded; ASTM D638
Elongation at Break 140 %140 %2.0 in/min, Injection Molded; ASTM D638
Elongation at Yield 9.2 %9.2 %2.0 in/min, Injection Molded; ASTM D638
Flexural Modulus, 1% Secant 1720 MPa249000 psiInjection Molded; ASTM D790A
Izod Impact, Notched 0.406 J/cm0.760 ft-lb/inInjection Molded; ASTM D256
Izod Impact, Notched (ISO) 3.40 kJ/m²1.62 ft-lb/in²Area, Injection Molded; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 65.0 °C149 °FUL Relative Thermal Index
Deflection Temperature at 0.46 MPa (66 psi) 104 °C220 °FUnannealed, Injection Molded; ASTM D648
UL RTI, Electrical 65.0 °C
@Thickness 3.05 mm
149 °F
@Thickness 0.120 in
UL 746
UL RTI, Mechanical with Impact 65.0 °C
@Thickness 3.05 mm
149 °F
@Thickness 0.120 in
UL 746
UL RTI, Mechanical without Impact 65.0 °C
@Thickness 3.05 mm
149 °F
@Thickness 0.120 in
UL 746
Flammability, UL94 HB
@Thickness 3.05 mm
HB
@Thickness 0.120 in
 
Optical PropertiesMetricEnglishComments
Haze 73 %
@Thickness 1.27 mm
73 %
@Thickness 0.0500 in
ASTM D1003
Gloss 93 %93 %60°; ASTM D2457
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Descriptive Properties
processExtrusion
 Injection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ineos H01G-00 Polypropylene Homopolymer
Ineos H05H-01 Polypropylene Homopolymer
Ineos H05M-00 Polypropylene Homopolymer
Ineos H07D-00 Polypropylene Homopolymer
Borealis RF926MO Polypropylene, Transparent Random Copolymer

PBPP28 / 27669

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.